ISO International Standard

Corrosion of metals and alloys — Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water

This document specifies a test method for determining the stress corrosion crack (SCC) growth rate of steels and alloys under static-load conditions in high-temperature water, such as the simulated water environment of light water reactors. The crack length of the specimen is monitored by a potential drop method (PDM) during the test in an autoclave.

The test method is applicable to stainless steels, nickel base alloys, low alloy steels, carbon steels and other alloys.

Purchase ISO Standard

$140.11

Share this Standard