ISO 15613:2004 specifies how a preliminary welding procedure specification is qualified based on pre-production welding tests.
It is applicable to arc welding, gas welding, beam welding, resistance welding, stud welding and friction welding of metallic materials.
The use of ISO 15613:2004 can be restricted by an application standard or specification.